2-D composites prepared from glassy fabric and siloxane resin as a matrix were cured and subjected to pyrolysis at 400, 500, 600.mult.C in nitrogen. Materials were oxidized in dried air at 400 and 700.mult.C for a period of 1h.
2-D composites prepared from glassy fabric and siloxane resin as a matrix were cured and subjected to pyrolysis at 400, 500, 600.mult.C in nitrogen. Materials were oxidized in dried air at 400 and 700.mult.C for a period of 1h. (en)