. "I" . "The pressure dependence of the saturation magnetization and Curie temperature was studied in melt-spun Fe60Mn20B20, Fe56Mn24B20 and Fe75B25 amorphous alloys up to 0.9 GPa, corresponding to volume changes up to 0.45%. In addition, in situ high-pressure (up to 40 GPa) x-ray diffraction was performed to determine the compressibility of the latter two alloys. Both the Curie temperature TC(at atmospheric pressure TC = 2013 and 1593 K)and the low-temperature saturation magnetization M5 K,5 T decrease remarkably with increasing pressure."@en . "Kamar\u00E1d, Ji\u0159\u00ED" . "Journal of Physics-Condensed Matter" . . "0953-8984" . . "[7380F981607F]" . "000322956200018" . "Kem\u00E9ny, T." . . "2"^^ . . . "Pressure dependence of magnetic properties in Fe\u2013Mn\u2013B amorphous alloys:evidence for inhomogeneous ferromagnetism"@en . "Konopkov\u00E1, Z." . "RIV/68378271:_____/13:00423907!RIV14-AV0-68378271" . . "34" . "7"^^ . . "Pressure dependence of magnetic properties in Fe\u2013Mn\u2013B amorphous alloys:evidence for inhomogeneous ferromagnetism"@en . "Pressure dependence of magnetic properties in Fe\u2013Mn\u2013B amorphous alloys:evidence for inhomogeneous ferromagnetism" . . . . "Bednar\u010D\u00EDk, J." . . "8"^^ . "magnetic properties; ferromagnetism"@en . "RIV/68378271:_____/13:00423907" . "Kiss, L. F." . . "99080" . "GB - Spojen\u00E9 kr\u00E1lovstv\u00ED Velk\u00E9 Brit\u00E1nie a Severn\u00EDho Irska" . "Liermann, H.-P." . "25" . "Pressure dependence of magnetic properties in Fe\u2013Mn\u2013B amorphous alloys:evidence for inhomogeneous ferromagnetism" . "10.1088/0953-8984/25/34/346002" . "The pressure dependence of the saturation magnetization and Curie temperature was studied in melt-spun Fe60Mn20B20, Fe56Mn24B20 and Fe75B25 amorphous alloys up to 0.9 GPa, corresponding to volume changes up to 0.45%. In addition, in situ high-pressure (up to 40 GPa) x-ray diffraction was performed to determine the compressibility of the latter two alloys. Both the Curie temperature TC(at atmospheric pressure TC = 2013 and 1593 K)and the low-temperature saturation magnetization M5 K,5 T decrease remarkably with increasing pressure." . . . "Arnold, Zden\u011Bk" .