. . "-" . . . "Preparation and properties of COx films" . "New types of amorphous graphite-like COx films, which contain at most 18-22% atomic oxygen were obtained. Two characteristic absorption bands at approximately 1700 and 1605 cm- 1. Only those films with 002 interlayer distance increased with respect to that of graphite may be saturated with oxygen up to approximately 22 at.%" . . "Preparation and properties of COx films"@en . . "4"^^ . . "Applied Physics A - Materials Science & Processing" . . "Preparation and properties of COx films"@en . "CO x films; magnetron sputtering; IR spectra; Raman spectra"@en . "RIV/68378271:_____/04:00100044" . "393;396" . "Preparation and properties of COx films" . "581533" . "6"^^ . "P\u0159\u00EDprava a vlastnosti vrstev COx./sub"@cs . . . "Kulykovskyy, Valeriy" . "Byly p\u0159ipraveny nov\u00E9 typy amorfn\u00EDch grafit\u016F podobn\u00FDch vrstev COx, je\u017E obsahuj\u00ED a\u017E 18 - 20 at. % kysl\u00EDku. Pozoruj\u00ED se dva charakteristick\u00E9 absorp\u010Dn\u00ED p\u00E1sy pobl\u00ED\u017E 1700 a 1605 cm- 1. Saturov\u00E1ny kysl\u00EDkem p\u0159ibli\u017En\u011B do 22 at. % mohou b\u00FDt pouze ty vrstvy, kde mezirovinn\u00E1 vzd\u00E1lenost (002) p\u0159evy\u0161uje vzd\u00E1lenost (002) v grafitu"@cs . "Boh\u00E1\u010D, Petr" . "[7170DD572D04]" . . "5"^^ . "Vorl\u00ED\u010Dek, Vladim\u00EDr" . "DE - Spolkov\u00E1 republika N\u011Bmecko" . . "0947-8396" . "Zemek, Josef" . . "Kurdyumov, A." . . . . "RIV/68378271:_____/04:00100044!RIV/2005/AV0/A02005/N" . "78" . . "Jastrab\u00EDk, Lubom\u00EDr" . . "P\u0159\u00EDprava a vlastnosti vrstev COx./sub"@cs . . "P(KSK2043105)" . "New types of amorphous graphite-like COx films, which contain at most 18-22% atomic oxygen were obtained. Two characteristic absorption bands at approximately 1700 and 1605 cm- 1. Only those films with 002 interlayer distance increased with respect to that of graphite may be saturated with oxygen up to approximately 22 at.%"@en . .