. "Low cycle fatigue of ferritic ductile cast iron with alloying nickel"@en . "Petrenec, Martin" . "Total strain controlled tests have been performed on cylindrical specimens of ductile cast iron with aim to assess of the fatigue resistance. Cyclic hardening, cyclic stress-strain and fatigue life curves were obtained. The microstructure is documented using light microscope. Fracture surface was studied using scanning electron microscopy. Manson-Coffin and Basquin laws can reasonably approximate the fatigue life data. Fatigue crack initiation close to the surface is documented."@en . . "[EA37143E76DE]" . . . "N\u00EDzkocyklov\u00E1 \u00FAnavov\u00E1 odolnost feritick\u00E9 litiny s kuli\u010Dkov\u00FDm grafitem legovan\u00E9 niklem" . "RIV/68081723:_____/08:00324454!RIV09-AV0-68081723" . . "N\u00EDzkocyklov\u00E1 \u00FAnavov\u00E1 odolnost feritick\u00E9 litiny s kuli\u010Dkov\u00FDm grafitem legovan\u00E9 niklem"@cs . "8"^^ . "Pacal, B." . . "Hradec nad Moravic\u00ED" . "2008-05-13+02:00"^^ . . . . "Low cycle fatigue of ferritic ductile cast iron with alloying nickel"@en . . "382774" . "3"^^ . . . "Ostrava" . "N\u00EDzkocyklov\u00E1 \u00FAnavov\u00E1 odolnost feritick\u00E9 litiny s kuli\u010Dkov\u00FDm grafitem legovan\u00E9 niklem"@cs . . "Tanger s.r.o." . . "Low cycle fatigue; FERRITIC ductile cast iron"@en . . "Zkou\u0161ky n\u00EDzkocyklov\u00E9 \u00FAnavy byly provedeny na v\u00E1lcov\u00FDch vzorc\u00EDch z litiny s kuli\u010Dkov\u00FDm grafitem (d\u00E1le LKG) v re\u017Eimu \u0159\u00EDzen\u00E9 deformace za \u00FA\u010Delem posouzen\u00ED \u00FAnavov\u00E9 odolnosti. Byly z\u00EDsk\u00E1ny k\u0159ivky cyklick\u00E9ho zpevn\u011Bn\u00ED, cyklick\u00E1 deforma\u010Dn\u00ED k\u0159ivka a k\u0159ivky \u00FAnavov\u00E9 \u017Eivotnosti. Je dokumentov\u00E1na mikrostruktura pomoc\u00ED sv\u011Bteln\u00E9 mikroskopie. Lomov\u00E1 plocha byla pozorov\u00E1na pomoc\u00ED elektronov\u00E9 rastrovac\u00ED mikroskopie. \u00DAnavovou \u017Eivotnost lze uspokojiv_ charakterizovat Manson-Coffinov\u00FDm a Basquinov\u00FDm z\u00E1konem. M\u00EDsta iniciace \u00FAnavov\u00FDch trhlin v bl\u00EDzkosti povrchu jsou zdokumentov\u00E1ny."@cs . . "N\u00EDzkocyklov\u00E1 \u00FAnavov\u00E1 odolnost feritick\u00E9 litiny s kuli\u010Dkov\u00FDm grafitem legovan\u00E9 niklem" . "1"^^ . "Tesa\u0159ov\u00E1, H." . "METAL 2008. Sborn\u00EDk p\u0159edn\u00E1\u0161ek." . "Zkou\u0161ky n\u00EDzkocyklov\u00E9 \u00FAnavy byly provedeny na v\u00E1lcov\u00FDch vzorc\u00EDch z litiny s kuli\u010Dkov\u00FDm grafitem (d\u00E1le LKG) v re\u017Eimu \u0159\u00EDzen\u00E9 deformace za \u00FA\u010Delem posouzen\u00ED \u00FAnavov\u00E9 odolnosti. Byly z\u00EDsk\u00E1ny k\u0159ivky cyklick\u00E9ho zpevn\u011Bn\u00ED, cyklick\u00E1 deforma\u010Dn\u00ED k\u0159ivka a k\u0159ivky \u00FAnavov\u00E9 \u017Eivotnosti. Je dokumentov\u00E1na mikrostruktura pomoc\u00ED sv\u011Bteln\u00E9 mikroskopie. Lomov\u00E1 plocha byla pozorov\u00E1na pomoc\u00ED elektronov\u00E9 rastrovac\u00ED mikroskopie. \u00DAnavovou \u017Eivotnost lze uspokojiv_ charakterizovat Manson-Coffinov\u00FDm a Basquinov\u00FDm z\u00E1konem. M\u00EDsta iniciace \u00FAnavov\u00FDch trhlin v bl\u00EDzkosti povrchu jsou zdokumentov\u00E1ny." . "P(1QS200410502), P(GD106/05/H008), Z(AV0Z20410507)" . "978-80-254-1987-8" . . "RIV/68081723:_____/08:00324454" . .