"In concrete structures such as bridges or tanks, hydro insulation is applied several months after the actual construction of the structure itself. Concrete structures dry during part of their lifespan throughout the entire area of their structure. After hydro insulation is applied, drying is affected and it does not occur as it would under normal conditions. This change in drying conditions can eventually lead to changes in the structural behaviour of the structure e.g. bridges or tanks."@en . "S" . "concrete, shrinkage, notional size of member, time dependent analysis"@en . . "21. BETON\u00C1\u0158SK\u00C9 DNY 2014 Sborn\u00EDk ke konferenci" . "\u010Cesk\u00E1 beton\u00E1\u0159sk\u00E1 spole\u010Dnost \u010CSSI" . "978-80-903806-7-7" . "2014-11-26+01:00"^^ . "527"^^ . "Zich, Milo\u0161" . "N\u00C1HRADN\u00CD ROZM\u011AR PR\u016E\u0158EZU A JEHO VLIV NA SMR\u0160\u0164OV\u00C1N\u00CD" . "RIV/00216305:26110/14:PU111501" . "31424" . "Hof\u00EDrek, Radovan" . "N\u00C1HRADN\u00CD ROZM\u011AR PR\u016E\u0158EZU A JEHO VLIV NA SMR\u0160\u0164OV\u00C1N\u00CD" . "26110" . . "[9929388B48A4]" . . . "Hradec kr\u00E1lov\u00E9" . "N\u00C1HRADN\u00CD ROZM\u011AR PR\u016E\u0158EZU A JEHO VLIV NA SMR\u0160\u0164OV\u00C1N\u00CD"@cs . . . "The effective cross-section thickness and its effect on shrinkage"@en . . "U betonov\u00FDch konstrukc\u00ED jako jsou mosty nebo n\u00E1dr\u017Ee se hydroizolace aplikuje s n\u011Bkolika m\u011Bs\u00ED\u010Dn\u00EDm zpo\u017Ed\u011Bn\u00EDm oproti vlastn\u00ED v\u00FDstavb\u011B betonov\u00E9ho pr\u016F\u0159ezu. Konstrukce \u010D\u00E1st sv\u00E9 \u017Eivotnosti vysych\u00E1 cel\u00FDm povrchem a po polo\u017Een\u00ED izolace br\u00E1n\u00EDc\u00ED vysych\u00E1n\u00ED pr\u016F\u0159ezu se zm\u011Bn\u00ED charakter zp\u016Fsobu vysych\u00E1n\u00ED. Tato zm\u011Bna m\u016F\u017Ee m\u00EDt za n\u00E1sledek zm\u011Bny chov\u00E1n\u00ED most\u016F nebo n\u00E1dr\u017E\u00ED." . . . . "U betonov\u00FDch konstrukc\u00ED jako jsou mosty nebo n\u00E1dr\u017Ee se hydroizolace aplikuje s n\u011Bkolika m\u011Bs\u00ED\u010Dn\u00EDm zpo\u017Ed\u011Bn\u00EDm oproti vlastn\u00ED v\u00FDstavb\u011B betonov\u00E9ho pr\u016F\u0159ezu. Konstrukce \u010D\u00E1st sv\u00E9 \u017Eivotnosti vysych\u00E1 cel\u00FDm povrchem a po polo\u017Een\u00ED izolace br\u00E1n\u00EDc\u00ED vysych\u00E1n\u00ED pr\u016F\u0159ezu se zm\u011Bn\u00ED charakter zp\u016Fsobu vysych\u00E1n\u00ED. Tato zm\u011Bna m\u016F\u017Ee m\u00EDt za n\u00E1sledek zm\u011Bny chov\u00E1n\u00ED most\u016F nebo n\u00E1dr\u017E\u00ED."@cs . "The effective cross-section thickness and its effect on shrinkage"@en . . . "2"^^ . "N\u00C1HRADN\u00CD ROZM\u011AR PR\u016E\u0158EZU A JEHO VLIV NA SMR\u0160\u0164OV\u00C1N\u00CD"@cs . . . . . . "Hradec Kr\u00E1lov\u00E9" . "RIV/00216305:26110/14:PU111501!RIV15-MSM-26110___" . "2"^^ .