"374734" . "1" . . . "Hlo\u017Eek, Martin" . . "2"^^ . "Geologick\u00E9 v\u00FDzkumy na Morav\u011B a ve Slezsku" . "Keramick\u00E1 petrografie lo\u0161tick\u00E9 hrn\u010Diny" . . "2"^^ . "Ceramic Petrography of Pottery from Lo\u0161tice"@en . . "4"^^ . "RIV/00216224:14310/08:00027433!RIV10-MSM-14310___" . . "The paper summarizes the results of micropetrographic examination of pottery from Lo\u0161tice. The burning temperature was experimentally verified. The results showed that (010), (020) and (030) pottery groups might have been made of the same, or very similar, plastic raw material with petrographically different non-plastics. The experiments showed that the burning temperature was reache 1200-1250 C."@en . "14310" . "CZ - \u010Cesk\u00E1 republika" . "Gregerov\u00E1, Miroslava" . . "V p\u0159\u00EDsp\u011Bvku jsou hrnuty v\u00FDsledky mikropetrografick\u00E9ho studia lo\u0161tick\u00FDch poh\u00E1r\u016F.teplota v\u00FDpalu byla ov\u011B\u0159ena experiment\u00E1ln\u011B. V\u00FDseldky ukazuj\u00ED \u017Ee poh\u00E1ry ze skupin (010),(020) a (030) mohly b\u00FDt vyr\u00E1b\u011Bny ze stejn\u00E9 nebo velmi podbn\u00E9 plastick\u00E9 suroviny s p\u0159\u00EDdavkem petrograficky odli\u0161n\u00E9ho ost\u0159iva. Experimenty uk\u00E1zaly, \u017Ee teplota v\u00FDpalu se pohybova mezi 1200 a\u017E 1250 st. C"@cs . . . "XV" . "1212-6209" . . "Keramick\u00E1 petrografie lo\u0161tick\u00E9 hrn\u010Diny" . "Keramick\u00E1 petrografie lo\u0161tick\u00E9 hrn\u010Diny"@cs . . "Keramick\u00E1 petrografie lo\u0161tick\u00E9 hrn\u010Diny"@cs . "[467DBF6619B8]" . "Ceramic Petrography of Pottery from Lo\u0161tice"@en . . "RIV/00216224:14310/08:00027433" . . "Pottery - technology - ceramic petrography - firing temperature"@en . "V p\u0159\u00EDsp\u011Bvku jsou hrnuty v\u00FDsledky mikropetrografick\u00E9ho studia lo\u0161tick\u00FDch poh\u00E1r\u016F.teplota v\u00FDpalu byla ov\u011B\u0159ena experiment\u00E1ln\u011B. V\u00FDseldky ukazuj\u00ED \u017Ee poh\u00E1ry ze skupin (010),(020) a (030) mohly b\u00FDt vyr\u00E1b\u011Bny ze stejn\u00E9 nebo velmi podbn\u00E9 plastick\u00E9 suroviny s p\u0159\u00EDdavkem petrograficky odli\u0161n\u00E9ho ost\u0159iva. Experimenty uk\u00E1zaly, \u017Ee teplota v\u00FDpalu se pohybova mezi 1200 a\u017E 1250 st. C" . . "Z(MSM0021622427)" .