| - An ethylene-octene copolymer (EOC) (45 wt% octene) is crosslinked using dicumyl peroxide (DCP). Differential scanning calorimetry (DSC) reveals a very low melting temperature (50 °C). The network density is evaluated by gel content. While 0.2-0.3 wt% of peroxide leads only to a molecular weight increase (samples completely dissolved in xylene), 0.4-0.6 wt% of peroxide caused network formation. High-temperature creep was measured at 70, 120, and 200 °C at three stress levels. At 200 °C and above 0.6 wt% of peroxide, degradation due to chain scission is observed by rubber process analyzer (RPA) and is again supported by creep measurements. Residual strain at 70 °C is found to improve with increasing peroxide level. Dynamic mechanical analysis (DMA) reveals a strong influence of peroxide content on storage modulus and tan δ, in particular in the range 30-200 °C.
- An ethylene-octene copolymer (EOC) (45 wt% octene) is crosslinked using dicumyl peroxide (DCP). Differential scanning calorimetry (DSC) reveals a very low melting temperature (50 °C). The network density is evaluated by gel content. While 0.2-0.3 wt% of peroxide leads only to a molecular weight increase (samples completely dissolved in xylene), 0.4-0.6 wt% of peroxide caused network formation. High-temperature creep was measured at 70, 120, and 200 °C at three stress levels. At 200 °C and above 0.6 wt% of peroxide, degradation due to chain scission is observed by rubber process analyzer (RPA) and is again supported by creep measurements. Residual strain at 70 °C is found to improve with increasing peroxide level. Dynamic mechanical analysis (DMA) reveals a strong influence of peroxide content on storage modulus and tan δ, in particular in the range 30-200 °C. (en)
|
Title
| - Creep and Dynamic mechanical analysis studies of peroxide-crosslinked ethylene-octene copolymer
- Creep and Dynamic mechanical analysis studies of peroxide-crosslinked ethylene-octene copolymer (en)
|
skos:prefLabel
| - Creep and Dynamic mechanical analysis studies of peroxide-crosslinked ethylene-octene copolymer
- Creep and Dynamic mechanical analysis studies of peroxide-crosslinked ethylene-octene copolymer (en)
|
skos:notation
| - RIV/70883521:28150/12:43867906!RIV13-MSM-28150___
|
http://linked.open...avai/predkladatel
| |
http://linked.open...avai/riv/aktivita
| |
http://linked.open...avai/riv/aktivity
| - P(ED2.1.00/03.0111), S, Z(MSM7088352102)
|
http://linked.open...iv/cisloPeriodika
| |
http://linked.open...vai/riv/dodaniDat
| |
http://linked.open...aciTvurceVysledku
| |
http://linked.open.../riv/druhVysledku
| |
http://linked.open...iv/duvernostUdaju
| |
http://linked.open...titaPredkladatele
| |
http://linked.open...dnocenehoVysledku
| |
http://linked.open...ai/riv/idVysledku
| - RIV/70883521:28150/12:43867906
|
http://linked.open...riv/jazykVysledku
| |
http://linked.open.../riv/klicovaSlova
| - peroxides; ethylene-octene copolymers; DMA; crosslinking; creep (en)
|
http://linked.open.../riv/klicoveSlovo
| |
http://linked.open...odStatuVydavatele
| - DE - Spolková republika Německo
|
http://linked.open...ontrolniKodProRIV
| |
http://linked.open...i/riv/nazevZdroje
| - Macromolecular Materials & Engineering
|
http://linked.open...in/vavai/riv/obor
| |
http://linked.open...ichTvurcuVysledku
| |
http://linked.open...cetTvurcuVysledku
| |
http://linked.open...vavai/riv/projekt
| |
http://linked.open...UplatneniVysledku
| |
http://linked.open...v/svazekPeriodika
| |
http://linked.open...iv/tvurceVysledku
| - Poongavalappil, Sameepa
- Svoboda, Petr
- Svobodová, Dagmar
- Theravalappil, Rajesh
|
http://linked.open...n/vavai/riv/zamer
| |
issn
| |
number of pages
| |
http://bibframe.org/vocab/doi
| |
http://localhost/t...ganizacniJednotka
| |
is http://linked.open...avai/riv/vysledek
of | |