Rychle ztuhlé slitiny Al-18wt%Ni připravené metodou rovinného lití na rotující CrZr kotouč. Teplota tání byla 2050°C, rychlost kotouče 30 s- 1. Pro porovnání byly též připraveny slitiny AlNi (cs)
AlNi17Zr1.8 was rapidly solidified (RS) by planar flow casting melt spinning on a rotating CrZr bronze wheel. The melt temperature was 2050°C, the wheet speed was 30 s- 1. For comparison AlNi18.5 alloy was also prepared
AlNi17Zr1.8 was rapidly solidified (RS) by planar flow casting melt spinning on a rotating CrZr bronze wheel. The melt temperature was 2050°C, the wheet speed was 30 s- 1. For comparison AlNi18.5 alloy was also prepared (en)