| - Polymide-Kapton (Pl) foils, 50 .mu.g thick were irradiated with 100 keV He.sup.+./sup., Ne.sup.+./sup., Ar.sup.+./sup.,Kr.sup.+./sup. and Xe.sup.+./sup. ions to the fluences from 1x10.sup.12./sup. to 1x10.sup.16./sup. cm.sup.-2./sup. and subsequently doped from 5 M/1 water solution of LiCl for 1 and 25 h at room temperature. The amount of incorporated LiCl dopant and its depth profiles were measured with non-destructive Neutron Depth Profiling (NDP) technique sensitive to sup.6./sup. Li isotope. The dopant uptake is a complikated function of the ion mass, ion fluence and the doping time. The depth profiles of the dopant in the PI samples irradiated to the fluences below 1x10.sup.13./sup. cm .sup.-2./sup. are similar to that from unirradiated PI. At higher fluences an anomalous profile component appears, the width of which correlates well with the ion projected range.
- Polymide-Kapton (Pl) foils, 50 .mu.g thick were irradiated with 100 keV He.sup.+./sup., Ne.sup.+./sup., Ar.sup.+./sup.,Kr.sup.+./sup. and Xe.sup.+./sup. ions to the fluences from 1x10.sup.12./sup. to 1x10.sup.16./sup. cm.sup.-2./sup. and subsequently doped from 5 M/1 water solution of LiCl for 1 and 25 h at room temperature. The amount of incorporated LiCl dopant and its depth profiles were measured with non-destructive Neutron Depth Profiling (NDP) technique sensitive to sup.6./sup. Li isotope. The dopant uptake is a complikated function of the ion mass, ion fluence and the doping time. The depth profiles of the dopant in the PI samples irradiated to the fluences below 1x10.sup.13./sup. cm .sup.-2./sup. are similar to that from unirradiated PI. At higher fluences an anomalous profile component appears, the width of which correlates well with the ion projected range. (en)
|
Title
| - Decoration of radiation damages in polyimide implanted with rare gas ions.
- Decoration of radiation damages in polyimide implanted with rare gas ions. (en)
|
skos:prefLabel
| - Decoration of radiation damages in polyimide implanted with rare gas ions.
- Decoration of radiation damages in polyimide implanted with rare gas ions. (en)
|
skos:notation
| - RIV/61389005:_____/02:49020070!RIV/2003/GA0/A49003/N
|
http://linked.open.../vavai/riv/strany
| |
http://linked.open...avai/riv/aktivita
| |
http://linked.open...avai/riv/aktivity
| - P(GA203/99/1626), P(IAA7011908), Z(AV0Z1048901)
|
http://linked.open...iv/cisloPeriodika
| |
http://linked.open...vai/riv/dodaniDat
| |
http://linked.open...aciTvurceVysledku
| |
http://linked.open.../riv/druhVysledku
| |
http://linked.open...iv/duvernostUdaju
| |
http://linked.open...titaPredkladatele
| |
http://linked.open...dnocenehoVysledku
| |
http://linked.open...ai/riv/idVysledku
| - RIV/61389005:_____/02:49020070
|
http://linked.open...riv/jazykVysledku
| |
http://linked.open.../riv/klicovaSlova
| - polyimide; ion implantation; doping neutron depth profiling (en)
|
http://linked.open.../riv/klicoveSlovo
| |
http://linked.open...odStatuVydavatele
| - US - Spojené státy americké
|
http://linked.open...ontrolniKodProRIV
| |
http://linked.open...i/riv/nazevZdroje
| - Surface and Coatings Technology
|
http://linked.open...in/vavai/riv/obor
| |
http://linked.open...ichTvurcuVysledku
| |
http://linked.open...cetTvurcuVysledku
| |
http://linked.open...ocetUcastnikuAkce
| |
http://linked.open...nichUcastnikuAkce
| |
http://linked.open...vavai/riv/projekt
| |
http://linked.open...UplatneniVysledku
| |
http://linked.open...v/svazekPeriodika
| |
http://linked.open...iv/tvurceVysledku
| - Hnatowicz, Vladimír
- Macková, Anna
- Vacík, Jiří
- Peřina, Vratislav
- Červená, Jarmila
- Fing, D.
|
http://linked.open...n/vavai/riv/zamer
| |
issn
| |
number of pages
| |