| - 50 mum thick polyimide (Kapton, PI) foils were irradiated with 100 keV He+, Ne+, Ar+ and Kr+ ions to fluences from 1 x 10(12) to 1 x 10(16) cm(-2), and the structural and compositional changes in the polymer surface layer, degraded by the ion bombardment, were studied by RES and ERDA techniques. The sheet resistance at room temperature was also measured. Significant hydrogen and oxygen depletion is observed for the ion fluences above 1 x 10(14) cm(-2) in the PIsurface layer, the thickness of which is an increasing function of the ion projected range. Measured H and O depth profiles are structureless with the concentration monotonically increasing from the sample surface to the sample bulk where it achieves the value typical for pristine PI. The sheet resistance remains unchanged up to the fluence of 10(14)cm(-2) and then it declines rapidly by several orders of magnitude, the decline being more pronounced for heavier ions.
- 50 mum thick polyimide (Kapton, PI) foils were irradiated with 100 keV He+, Ne+, Ar+ and Kr+ ions to fluences from 1 x 10(12) to 1 x 10(16) cm(-2), and the structural and compositional changes in the polymer surface layer, degraded by the ion bombardment, were studied by RES and ERDA techniques. The sheet resistance at room temperature was also measured. Significant hydrogen and oxygen depletion is observed for the ion fluences above 1 x 10(14) cm(-2) in the PIsurface layer, the thickness of which is an increasing function of the ion projected range. Measured H and O depth profiles are structureless with the concentration monotonically increasing from the sample surface to the sample bulk where it achieves the value typical for pristine PI. The sheet resistance remains unchanged up to the fluence of 10(14)cm(-2) and then it declines rapidly by several orders of magnitude, the decline being more pronounced for heavier ions. (en)
|
Title
| - Degradation of polyimide by 100 keV He+, Ne+, Ar+ and Kr+ ions.
- Degradation of polyimide by 100 keV He+, Ne+, Ar+ and Kr+ ions. (en)
|
skos:prefLabel
| - Degradation of polyimide by 100 keV He+, Ne+, Ar+ and Kr+ ions.
- Degradation of polyimide by 100 keV He+, Ne+, Ar+ and Kr+ ions. (en)
|
skos:notation
| - RIV/61389005:_____/01:49010049!RIV/2003/AV0/A49003/N
|
http://linked.open.../vavai/riv/strany
| |
http://linked.open...avai/riv/aktivita
| |
http://linked.open...avai/riv/aktivity
| - P(GA203/99/1626), P(IAA7011908), P(KSK1010104), Z(AV0Z1048901)
|
http://linked.open...iv/cisloPeriodika
| |
http://linked.open...vai/riv/dodaniDat
| |
http://linked.open...aciTvurceVysledku
| |
http://linked.open.../riv/druhVysledku
| |
http://linked.open...iv/duvernostUdaju
| |
http://linked.open...titaPredkladatele
| |
http://linked.open...dnocenehoVysledku
| |
http://linked.open...ai/riv/idVysledku
| - RIV/61389005:_____/01:49010049
|
http://linked.open...riv/jazykVysledku
| |
http://linked.open.../riv/klicovaSlova
| |
http://linked.open.../riv/klicoveSlovo
| |
http://linked.open...odStatuVydavatele
| |
http://linked.open...ontrolniKodProRIV
| |
http://linked.open...i/riv/nazevZdroje
| - Nuclear Instruments and Methods in Physics Research. B - Beam Interactions with Materials and Atoms
|
http://linked.open...in/vavai/riv/obor
| |
http://linked.open...ichTvurcuVysledku
| |
http://linked.open...cetTvurcuVysledku
| |
http://linked.open...ocetUcastnikuAkce
| |
http://linked.open...nichUcastnikuAkce
| |
http://linked.open...vavai/riv/projekt
| |
http://linked.open...UplatneniVysledku
| |
http://linked.open...v/svazekPeriodika
| |
http://linked.open...iv/tvurceVysledku
| - Heitz, J.
- Hnatowicz, Vladimír
- Macková, Anna
- Peřina, Vratislav
- Švorčík, V.
- Rybka, V.
- Fink, V.
|
http://linked.open...n/vavai/riv/zamer
| |
issn
| |
number of pages
| |