  • Analyses of Art Nouveau mosaics from the church of St. Simon and Juda in Dolín near Slaný and from Holovousy, both most likely made by the workshop of Viktor Foerster, have shown that the author used the NaO-PbO-SiO 22 glass type and that he used the same glass also for restoration of The Last Judgment mosaic at the Prague Castle in 1890-1910. Despite the fact that lead glasses are more durable than potassium glasses, the material investigations identified corrosion processes on the surface of the glass pieces (tesserae) depending on their composition. Apart from the analyzed mosaic NaO-PbO-SiO2 glasses, we also used ancient sodium glasses (NaO-CaO-SiO2) and 22 potassium glasses (K2O-CaO-SiO2) from archaeological finds in Opava to demonstrate their different chemical durability. We also paid attention to fixation binders used in Art Nouveau mosaics. Inappropriate use of gypsum-containing binders is a significant cause of disintegration of the mosaics. Gypsum and gypsum-lime plasters are very sensitive to humidity. Capillary action of water is a very serious problem that endangers the overall lifespan of any mosaic.
  • Analyses of Art Nouveau mosaics from the church of St. Simon and Juda in Dolín near Slaný and from Holovousy, both most likely made by the workshop of Viktor Foerster, have shown that the author used the NaO-PbO-SiO 22 glass type and that he used the same glass also for restoration of The Last Judgment mosaic at the Prague Castle in 1890-1910. Despite the fact that lead glasses are more durable than potassium glasses, the material investigations identified corrosion processes on the surface of the glass pieces (tesserae) depending on their composition. Apart from the analyzed mosaic NaO-PbO-SiO2 glasses, we also used ancient sodium glasses (NaO-CaO-SiO2) and 22 potassium glasses (K2O-CaO-SiO2) from archaeological finds in Opava to demonstrate their different chemical durability. We also paid attention to fixation binders used in Art Nouveau mosaics. Inappropriate use of gypsum-containing binders is a significant cause of disintegration of the mosaics. Gypsum and gypsum-lime plasters are very sensitive to humidity. Capillary action of water is a very serious problem that endangers the overall lifespan of any mosaic. (en)
Title
  • Signs of degradation of czech art nouveau mosaic glasses
  • Signs of degradation of czech art nouveau mosaic glasses (en)
skos:prefLabel
  • Signs of degradation of czech art nouveau mosaic glasses
  • Signs of degradation of czech art nouveau mosaic glasses (en)
skos:notation
  • RIV/61388980:_____/12:00390201!RIV13-AV0-61388980
http://linked.open...avai/predkladatel
http://linked.open...avai/riv/aktivita
http://linked.open...avai/riv/aktivity
  • I
http://linked.open...vai/riv/dodaniDat
http://linked.open...aciTvurceVysledku
http://linked.open.../riv/druhVysledku
http://linked.open...iv/duvernostUdaju
http://linked.open...titaPredkladatele
http://linked.open...dnocenehoVysledku
  • 167832
http://linked.open...ai/riv/idVysledku
  • RIV/61388980:_____/12:00390201
http://linked.open...riv/jazykVysledku
http://linked.open.../riv/klicovaSlova
  • glass mosaic; tesserae; glass corrosion; Victor Foerster; lead glass; Art Nouveau (en)
http://linked.open.../riv/klicoveSlovo
http://linked.open...ontrolniKodProRIV
  • [9EF12C540CC4]
http://linked.open...v/mistoKonaniAkce
  • Praha
http://linked.open...i/riv/mistoVydani
  • PRAHA
http://linked.open...i/riv/nazevZdroje
  • ACTA ARTIS ACADEMICA 2012: KNOWLEDGE AND EXPERIENCE IN THE FINE ART
http://linked.open...in/vavai/riv/obor
http://linked.open...ichTvurcuVysledku
http://linked.open...cetTvurcuVysledku
http://linked.open...UplatneniVysledku
http://linked.open...iv/tvurceVysledku
  • Hájek, T.
  • Švarcová, Silvie
  • Rohanová, D.
http://linked.open...vavai/riv/typAkce
http://linked.open...ain/vavai/riv/wos
  • 000313137700013
http://linked.open.../riv/zahajeniAkce
number of pages
http://purl.org/ne...btex#hasPublisher
  • Akademie výtvarných umění v Praze
https://schema.org/isbn
  • 978-80-87108-33-8
is http://linked.open...avai/riv/vysledek of
Faceted Search & Find service v1.16.118 as of Jun 21 2024


Alternative Linked Data Documents: ODE     Content Formats:   [cxml] [csv]     RDF   [text] [turtle] [ld+json] [rdf+json] [rdf+xml]     ODATA   [atom+xml] [odata+json]     Microdata   [microdata+json] [html]    About   
This material is Open Knowledge   W3C Semantic Web Technology [RDF Data] Valid XHTML + RDFa
OpenLink Virtuoso version 07.20.3240 as of Jun 21 2024, on Linux (x86_64-pc-linux-gnu), Single-Server Edition (126 GB total memory, 58 GB memory in use)
Data on this page belongs to its respective rights holders.
Virtuoso Faceted Browser Copyright © 2009-2024 OpenLink Software