  • Alumina-zirconia composite ceramics (AZ composites) have been prepared in the whole range of compositions from pure alumina to zirconia (in steps of 10 vol.%) by slip casting, followed by sintering at 1350 °C and microstructural characterization via the Archimedes method (relative densities 0.93-0.99). Young's modulus has been measured at room temperature via the impulse excitation technique (IET) and, after appropriate porosity correction (linear, power-law, exponential), found to be in good agreement with the Hashin-Shtrikman bounds. The damping factor (internal friction), which has been measured for dense AZ composites (also via IET at room temperature), is found to increase with increasing zirconia content. Damping factors measured for porous AZ composites with porosities 25-71 %, prepared with corn starch as a pore former, have been found to depend only slightly on porosity, unless the porosities are extremely high (} 70 %). At these porosities, however, where the Young's moduli approach zero, the damping factors exhibit a steep increase.
  • Alumina-zirconia composite ceramics (AZ composites) have been prepared in the whole range of compositions from pure alumina to zirconia (in steps of 10 vol.%) by slip casting, followed by sintering at 1350 °C and microstructural characterization via the Archimedes method (relative densities 0.93-0.99). Young's modulus has been measured at room temperature via the impulse excitation technique (IET) and, after appropriate porosity correction (linear, power-law, exponential), found to be in good agreement with the Hashin-Shtrikman bounds. The damping factor (internal friction), which has been measured for dense AZ composites (also via IET at room temperature), is found to increase with increasing zirconia content. Damping factors measured for porous AZ composites with porosities 25-71 %, prepared with corn starch as a pore former, have been found to depend only slightly on porosity, unless the porosities are extremely high (} 70 %). At these porosities, however, where the Young's moduli approach zero, the damping factors exhibit a steep increase. (en)
Title
  • Elastic properties and damping behavior of alumina-zirconia composites at room temperature
  • Elastic properties and damping behavior of alumina-zirconia composites at room temperature (en)
skos:prefLabel
  • Elastic properties and damping behavior of alumina-zirconia composites at room temperature
  • Elastic properties and damping behavior of alumina-zirconia composites at room temperature (en)
skos:notation
  • RIV/60461373:22310/12:43894493!RIV13-GA0-22310___
http://linked.open...avai/predkladatel
http://linked.open...avai/riv/aktivita
http://linked.open...avai/riv/aktivity
  • P(GAP108/12/1170)
http://linked.open...iv/cisloPeriodika
  • 7
http://linked.open...vai/riv/dodaniDat
http://linked.open...aciTvurceVysledku
http://linked.open.../riv/druhVysledku
http://linked.open...iv/duvernostUdaju
http://linked.open...titaPredkladatele
http://linked.open...dnocenehoVysledku
  • 133782
http://linked.open...ai/riv/idVysledku
  • RIV/60461373:22310/12:43894493
http://linked.open...riv/jazykVysledku
http://linked.open.../riv/klicovaSlova
  • porous ceramics (porosity); mechanical damping; elastic moduli (Young's modulus); alumina-zirconia composites; zirconia; Alumina (en)
http://linked.open.../riv/klicoveSlovo
http://linked.open...odStatuVydavatele
  • BE - Belgické království
http://linked.open...ontrolniKodProRIV
  • [6318C1C01B9C]
http://linked.open...i/riv/nazevZdroje
  • Ceramics International
http://linked.open...in/vavai/riv/obor
http://linked.open...ichTvurcuVysledku
http://linked.open...cetTvurcuVysledku
http://linked.open...vavai/riv/projekt
http://linked.open...UplatneniVysledku
http://linked.open...v/svazekPeriodika
  • 38
http://linked.open...iv/tvurceVysledku
  • Gregorová, Eva
  • Pabst, Willi
  • Hostaša, Jan
  • Malangré, Daniel
issn
  • 0272-8842
number of pages
http://bibframe.org/vocab/doi
  • 10.1016/j.ceramint.2012.04.045
http://localhost/t...ganizacniJednotka
  • 22310
is http://linked.open...avai/riv/vysledek of
Faceted Search & Find service v1.16.118 as of Jun 21 2024


Alternative Linked Data Documents: ODE     Content Formats:   [cxml] [csv]     RDF   [text] [turtle] [ld+json] [rdf+json] [rdf+xml]     ODATA   [atom+xml] [odata+json]     Microdata   [microdata+json] [html]    About   
This material is Open Knowledge   W3C Semantic Web Technology [RDF Data] Valid XHTML + RDFa
OpenLink Virtuoso version 07.20.3240 as of Jun 21 2024, on Linux (x86_64-pc-linux-gnu), Single-Server Edition (126 GB total memory, 58 GB memory in use)
Data on this page belongs to its respective rights holders.
Virtuoso Faceted Browser Copyright © 2009-2024 OpenLink Software