  • Structure and properties of magnesium can be modified by addition of solutes as well as by the metal working operations. To elucidate the alloying effect on both the deformation and the recrystallization mechanism, the present work compares the development of the microstructures of Mg-4Zn and Mg-4Zn-0.4Ca alloys (in wt.%) processed via two different deformation processes: the uniaxial compression (UC) and the equal channel angular pressing (ECAP). The stress-strain curves exhibited the classic evolution with the strain rate sensitivity slightly higher for Mg-4Zn than for Mg-4Zn-0.4Ca whereas the absolute value of the stress was higher in case of the ternary alloy during two deformation processes. Microstructure analysis showed that the hot deformation resulted generally in formation of the bimodal structure composed of fine grains of several micrometers and coarse unrecrystallized grains. Moreover, lower strain rates condition led to deformation-induced precipitation. The aim of the current work is therefore to better describe the effect of the Ca addition into Mg-4Zn alloy on its deformation as well as to reveal the mechanism(s) of the recrystallization phenomenon observed in such alloys.
  • Structure and properties of magnesium can be modified by addition of solutes as well as by the metal working operations. To elucidate the alloying effect on both the deformation and the recrystallization mechanism, the present work compares the development of the microstructures of Mg-4Zn and Mg-4Zn-0.4Ca alloys (in wt.%) processed via two different deformation processes: the uniaxial compression (UC) and the equal channel angular pressing (ECAP). The stress-strain curves exhibited the classic evolution with the strain rate sensitivity slightly higher for Mg-4Zn than for Mg-4Zn-0.4Ca whereas the absolute value of the stress was higher in case of the ternary alloy during two deformation processes. Microstructure analysis showed that the hot deformation resulted generally in formation of the bimodal structure composed of fine grains of several micrometers and coarse unrecrystallized grains. Moreover, lower strain rates condition led to deformation-induced precipitation. The aim of the current work is therefore to better describe the effect of the Ca addition into Mg-4Zn alloy on its deformation as well as to reveal the mechanism(s) of the recrystallization phenomenon observed in such alloys. (en)
Title
  • Microstructure development of Ca-doped Mg-Zn alloy during hot deformation
  • Microstructure development of Ca-doped Mg-Zn alloy during hot deformation (en)
skos:prefLabel
  • Microstructure development of Ca-doped Mg-Zn alloy during hot deformation
  • Microstructure development of Ca-doped Mg-Zn alloy during hot deformation (en)
skos:notation
  • RIV/60461373:22310/12:43894429!RIV13-MSM-22310___
http://linked.open...avai/predkladatel
http://linked.open...avai/riv/aktivita
http://linked.open...avai/riv/aktivity
  • P(KAN300100801), S
http://linked.open...vai/riv/dodaniDat
http://linked.open...aciTvurceVysledku
http://linked.open.../riv/druhVysledku
http://linked.open...iv/duvernostUdaju
http://linked.open...titaPredkladatele
http://linked.open...dnocenehoVysledku
  • 150431
http://linked.open...ai/riv/idVysledku
  • RIV/60461373:22310/12:43894429
http://linked.open...riv/jazykVysledku
http://linked.open.../riv/klicovaSlova
  • microstructure; recrystallization; deformation; Magnesium alloys (en)
http://linked.open.../riv/klicoveSlovo
http://linked.open...ontrolniKodProRIV
  • [49FE3A1888F0]
http://linked.open...v/mistoKonaniAkce
  • Brno
http://linked.open...i/riv/mistoVydani
  • Ostrava
http://linked.open...i/riv/nazevZdroje
  • Proceedings of 21st International Conference on Metallurgy and Materials
http://linked.open...in/vavai/riv/obor
http://linked.open...ichTvurcuVysledku
http://linked.open...cetTvurcuVysledku
http://linked.open...vavai/riv/projekt
http://linked.open...UplatneniVysledku
http://linked.open...iv/tvurceVysledku
  • Lejček, Pavel
  • Hradilová, Monika
  • Desrayaud, Christophe
  • Fraczkiewicz, Fraczkiewicz
  • Montheille, Frank
http://linked.open...vavai/riv/typAkce
http://linked.open...ain/vavai/riv/wos
  • 000318506500184
http://linked.open.../riv/zahajeniAkce
number of pages
http://purl.org/ne...btex#hasPublisher
  • TANGER
https://schema.org/isbn
  • 978-80-87294-29-1
http://localhost/t...ganizacniJednotka
  • 22310
is http://linked.open...avai/riv/vysledek of
Faceted Search & Find service v1.16.118 as of Jun 21 2024


Alternative Linked Data Documents: ODE     Content Formats:   [cxml] [csv]     RDF   [text] [turtle] [ld+json] [rdf+json] [rdf+xml]     ODATA   [atom+xml] [odata+json]     Microdata   [microdata+json] [html]    About   
This material is Open Knowledge   W3C Semantic Web Technology [RDF Data] Valid XHTML + RDFa
OpenLink Virtuoso version 07.20.3240 as of Jun 21 2024, on Linux (x86_64-pc-linux-gnu), Single-Server Edition (126 GB total memory, 58 GB memory in use)
Data on this page belongs to its respective rights holders.
Virtuoso Faceted Browser Copyright © 2009-2024 OpenLink Software