Both the static and dynamic corrosion tests of E-glass were used for different conditions. Results obtained for glass fibres were compared with the ones for glass grains and planar samples.
Both the static and dynamic corrosion tests of E-glass were used for different conditions. Results obtained for glass fibres were compared with the ones for glass grains and planar samples. (en)
Jak statické tak dynamické korozní testy E- skla byly použity pro různé podmínky. Výsledky získané pro skleněná vlákna byly srovnány s výsledky pro skleněná zrnka a ploché vzorky. (cs)