| - The paper deals with hypothesis of initiation and propagation of transverse crack verified by behaviour of tensile test samples taken from continuously cast slab of similar chemical composition within the temperature range from 25°C to 1450°C. In this manner it is possible to particularise and verify mechanism of initiation and subsequent discrete propagation of transverse crack, to evaluate temperature interval in which initiation of transverse crack was of the highest probability and to assess also to what degree anomalies in applied continuous casting technology could have influenced initiation of transverse crack.
- The paper deals with hypothesis of initiation and propagation of transverse crack verified by behaviour of tensile test samples taken from continuously cast slab of similar chemical composition within the temperature range from 25°C to 1450°C. In this manner it is possible to particularise and verify mechanism of initiation and subsequent discrete propagation of transverse crack, to evaluate temperature interval in which initiation of transverse crack was of the highest probability and to assess also to what degree anomalies in applied continuous casting technology could have influenced initiation of transverse crack. (en)
- Možnosti verifikace mechanismu vzniku příčné trhliny v CC ocelové bramě (cs)
|
Title
| - On the possibilities of verifying the cross cracking mechanism in the con-cast steel slab
- On the possibilities of verifying the cross cracking mechanism in the con-cast steel slab (en)
- Možnosti verifikace mechanismu vzniku příčné trhliny v CC ocelové bramě (cs)
|
skos:prefLabel
| - On the possibilities of verifying the cross cracking mechanism in the con-cast steel slab
- On the possibilities of verifying the cross cracking mechanism in the con-cast steel slab (en)
- Možnosti verifikace mechanismu vzniku příčné trhliny v CC ocelové bramě (cs)
|
skos:notation
| - RIV/61989100:27360/04:00010129!RIV/2005/GA0/273605/N
|
http://linked.open.../vavai/riv/strany
| |
http://linked.open...avai/riv/aktivita
| |
http://linked.open...avai/riv/aktivity
| - P(GA106/03/0264), Z(MSM 273600002)
|
http://linked.open...vai/riv/dodaniDat
| |
http://linked.open...aciTvurceVysledku
| |
http://linked.open.../riv/druhVysledku
| |
http://linked.open...iv/duvernostUdaju
| |
http://linked.open...titaPredkladatele
| |
http://linked.open...dnocenehoVysledku
| |
http://linked.open...ai/riv/idVysledku
| - RIV/61989100:27360/04:00010129
|
http://linked.open...riv/jazykVysledku
| |
http://linked.open.../riv/klicovaSlova
| - continuously cast steel slab;tensile test;transverse crack (en)
|
http://linked.open.../riv/klicoveSlovo
| |
http://linked.open...ontrolniKodProRIV
| |
http://linked.open...v/mistoKonaniAkce
| |
http://linked.open...i/riv/mistoVydani
| |
http://linked.open...i/riv/nazevZdroje
| - Damage and Fracture Mechanics
|
http://linked.open...in/vavai/riv/obor
| |
http://linked.open...ichTvurcuVysledku
| |
http://linked.open...cetTvurcuVysledku
| |
http://linked.open...vavai/riv/projekt
| |
http://linked.open...UplatneniVysledku
| |
http://linked.open...iv/tvurceVysledku
| - Dobrovská, Jana
- Kavička, František
- Stránský, Karel
- Dobrovská, Věra
- Štětina, J.
- Heger, J.
- Blaštíková, J.
|
http://linked.open...vavai/riv/typAkce
| |
http://linked.open.../riv/zahajeniAkce
| |
http://linked.open...n/vavai/riv/zamer
| |
number of pages
| |
http://purl.org/ne...btex#hasPublisher
| |
https://schema.org/isbn
| |
http://localhost/t...ganizacniJednotka
| |