  • The effects of annealing on gold structures sputtered onto glass substrate were studied using AFM, UV-Vis methods and electrical measurements. The colour of the as-deposited films changes from blue to green with increasing deposition time. After 1 hour annealing at 300 degrees C the structures acquire red colour regardless of the film thickness. The annealing results in dramatic changes of surface morphology and roughness and creation of relatively large %22spherolytic and hummock-like%22 structures in the gold layer. For deposited structures a non-zero optical band gap E(g)(opt) was determined from UV-Vis spectra using Tauc's model and it indicates a semi-conducting character of the structures. The annealing leads to an increase of the band gap. Electrical resistance of the deposited unannealed structures decreases dramatically for deposition times above 50 s. For annealed structures the resistance fall comes until after 250 s deposition time.
  • The effects of annealing on gold structures sputtered onto glass substrate were studied using AFM, UV-Vis methods and electrical measurements. The colour of the as-deposited films changes from blue to green with increasing deposition time. After 1 hour annealing at 300 degrees C the structures acquire red colour regardless of the film thickness. The annealing results in dramatic changes of surface morphology and roughness and creation of relatively large %22spherolytic and hummock-like%22 structures in the gold layer. For deposited structures a non-zero optical band gap E(g)(opt) was determined from UV-Vis spectra using Tauc's model and it indicates a semi-conducting character of the structures. The annealing leads to an increase of the band gap. Electrical resistance of the deposited unannealed structures decreases dramatically for deposition times above 50 s. For annealed structures the resistance fall comes until after 250 s deposition time. (en)
Title
  • Annealing of sputtered gold nano-structures
  • Annealing of sputtered gold nano-structures (en)
skos:prefLabel
  • Annealing of sputtered gold nano-structures
  • Annealing of sputtered gold nano-structures (en)
skos:notation
  • RIV/60461373:22310/11:43892540!RIV12-MSM-22310___
http://linked.open...avai/riv/aktivita
http://linked.open...avai/riv/aktivity
  • P(GA106/09/0125), P(GAP108/10/1106), P(IAA400720710), P(KAN200100801), P(KAN400480701), P(LC06041)
http://linked.open...iv/cisloPeriodika
  • 3
http://linked.open...vai/riv/dodaniDat
http://linked.open...aciTvurceVysledku
http://linked.open.../riv/druhVysledku
http://linked.open...iv/duvernostUdaju
http://linked.open...titaPredkladatele
http://linked.open...dnocenehoVysledku
  • 186326
http://linked.open...ai/riv/idVysledku
  • RIV/60461373:22310/11:43892540
http://linked.open...riv/jazykVysledku
http://linked.open.../riv/klicovaSlova
  • surface properties; AFM; Au nano-structures; sputtering; Annealing (en)
http://linked.open.../riv/klicoveSlovo
http://linked.open...odStatuVydavatele
  • US - Spojené státy americké
http://linked.open...ontrolniKodProRIV
  • [E07599A52BB4]
http://linked.open...i/riv/nazevZdroje
  • Applied Physics A-Materials Science & Processing
http://linked.open...in/vavai/riv/obor
http://linked.open...ichTvurcuVysledku
http://linked.open...cetTvurcuVysledku
http://linked.open...vavai/riv/projekt
http://linked.open...UplatneniVysledku
http://linked.open...v/svazekPeriodika
  • 102
http://linked.open...iv/tvurceVysledku
  • Kolská, Zdeňka
  • Kvítek, Ondřej
  • Lyutakov, Oleksiy
  • Siegel, Jakub
  • Švorčík, Václav
http://linked.open...ain/vavai/riv/wos
  • 000287320600035
issn
  • 0947-8396
number of pages
http://bibframe.org/vocab/doi
  • 10.1007/s00339-010-5977-5
http://localhost/t...ganizacniJednotka
  • 22310
Faceted Search & Find service v1.16.118 as of Jun 21 2024


Alternative Linked Data Documents: ODE     Content Formats:   [cxml] [csv]     RDF   [text] [turtle] [ld+json] [rdf+json] [rdf+xml]     ODATA   [atom+xml] [odata+json]     Microdata   [microdata+json] [html]    About   
This material is Open Knowledge   W3C Semantic Web Technology [RDF Data] Valid XHTML + RDFa
OpenLink Virtuoso version 07.20.3240 as of Jun 21 2024, on Linux (x86_64-pc-linux-gnu), Single-Server Edition (126 GB total memory, 58 GB memory in use)
Data on this page belongs to its respective rights holders.
Virtuoso Faceted Browser Copyright © 2009-2024 OpenLink Software