Attributes | Values |
---|
rdf:type
| |
Description
| - Wooden constructions and their parts in the exterior, e.g. houses, cottages, bowers, bridges, claddings, decking, windows or garden furniture, are degradable by bio-agencies, fire and weathering. Their service life can be increased by well-designed construction systems, by using of more durable wood species and composite materials, and also by convenient biocides and antiweathering paints. In experiments, the colour changes (valued by CIELab) and surface defects (valued at 10x magnification) in wood samples during their 3-year’s outdoor weathering at 45° were determined in an accordance with the EN 927-3 2000, taking into account these variable factors: 1) two wood species (black locust, Norway spruce); 2) four transparent coating systems (PerlColor, PerlColor + AquaStop, OsmoUV-Protection Oil 420, OsmoUV-Protection Oil 420 + AquaStop); 3) two roughness of wood (grinded with 60 or 120 sandpaper). Generally at natural weathering, the colours of the black locust wood untreated and treated wit
- Wooden constructions and their parts in the exterior, e.g. houses, cottages, bowers, bridges, claddings, decking, windows or garden furniture, are degradable by bio-agencies, fire and weathering. Their service life can be increased by well-designed construction systems, by using of more durable wood species and composite materials, and also by convenient biocides and antiweathering paints. In experiments, the colour changes (valued by CIELab) and surface defects (valued at 10x magnification) in wood samples during their 3-year’s outdoor weathering at 45° were determined in an accordance with the EN 927-3 2000, taking into account these variable factors: 1) two wood species (black locust, Norway spruce); 2) four transparent coating systems (PerlColor, PerlColor + AquaStop, OsmoUV-Protection Oil 420, OsmoUV-Protection Oil 420 + AquaStop); 3) two roughness of wood (grinded with 60 or 120 sandpaper). Generally at natural weathering, the colours of the black locust wood untreated and treated wit (en)
|
Title
| - COLOUR STABILITY AND SURFACE DEFECTS OF NATURALLY AGED WOOD TREATED WITH TRANSPARENT PAINTS FOR EXTERIOR CONSTRUCTIONS
- COLOUR STABILITY AND SURFACE DEFECTS OF NATURALLY AGED WOOD TREATED WITH TRANSPARENT PAINTS FOR EXTERIOR CONSTRUCTIONS (en)
|
skos:prefLabel
| - COLOUR STABILITY AND SURFACE DEFECTS OF NATURALLY AGED WOOD TREATED WITH TRANSPARENT PAINTS FOR EXTERIOR CONSTRUCTIONS
- COLOUR STABILITY AND SURFACE DEFECTS OF NATURALLY AGED WOOD TREATED WITH TRANSPARENT PAINTS FOR EXTERIOR CONSTRUCTIONS (en)
|
skos:notation
| - RIV/60460709:41320/14:64116!RIV15-MSM-41320___
|
http://linked.open...avai/riv/aktivita
| |
http://linked.open...avai/riv/aktivity
| |
http://linked.open...iv/cisloPeriodika
| |
http://linked.open...vai/riv/dodaniDat
| |
http://linked.open...aciTvurceVysledku
| |
http://linked.open.../riv/druhVysledku
| |
http://linked.open...iv/duvernostUdaju
| |
http://linked.open...titaPredkladatele
| |
http://linked.open...dnocenehoVysledku
| |
http://linked.open...ai/riv/idVysledku
| - RIV/60460709:41320/14:64116
|
http://linked.open...riv/jazykVysledku
| |
http://linked.open.../riv/klicovaSlova
| - Construction wood, paints, weathering, colour stability, surface defects (en)
|
http://linked.open.../riv/klicoveSlovo
| |
http://linked.open...odStatuVydavatele
| |
http://linked.open...ontrolniKodProRIV
| |
http://linked.open...i/riv/nazevZdroje
| |
http://linked.open...in/vavai/riv/obor
| |
http://linked.open...ichTvurcuVysledku
| |
http://linked.open...cetTvurcuVysledku
| |
http://linked.open...UplatneniVysledku
| |
http://linked.open...v/svazekPeriodika
| |
http://linked.open...iv/tvurceVysledku
| - Reinprecht, Ladislav
- Pánek, Miloš
|
http://linked.open...ain/vavai/riv/wos
| |
issn
| |
number of pages
| |
http://localhost/t...ganizacniJednotka
| |