Permitivita v závislosti na teplotě byla studována na 1000 nm silných filmech připravených z roztoku PMMA dopovaného 20 wt.% diphenyl sulfoxidu. (cs)
Permittivity of about 1000 nm thick films prepared from PMMA solution doped with 20 wt.% of diphenyl sulfoxide was studied as a function of temperature.
Permittivity of about 1000 nm thick films prepared from PMMA solution doped with 20 wt.% of diphenyl sulfoxide was studied as a function of temperature. (en)