| - The thermal degradation of polyaniline films polymerized in situ on silicon windows, and protonated with hydrochloric, sulfuric, or phosphoric acid, has been studied by FTIR spectroscopy. The conductivity decrease and spectral shifts induced by thermal ageing at 150 °C have been examined and are discussed in terms of deprotonation. Other chemical changes and the nature of the structural modifications introduced during thermal treatment have been interpreted using FTIR spectroscopy.
- The thermal degradation of polyaniline films polymerized in situ on silicon windows, and protonated with hydrochloric, sulfuric, or phosphoric acid, has been studied by FTIR spectroscopy. The conductivity decrease and spectral shifts induced by thermal ageing at 150 °C have been examined and are discussed in terms of deprotonation. Other chemical changes and the nature of the structural modifications introduced during thermal treatment have been interpreted using FTIR spectroscopy. (en)
- Teplotní degradace polyanilinových filmů polymerizovaných in situ na křemíkových okénkách a protonovaných kyselinou chlorovodíkovou, sírovou a fosforečnou byla studována pomocí FTIR spektroskopie. Byl studován a diskutován pokles vodivosti a spektrální posuny vlivem teplotního působení při 150 °C v souvislosti s deprotonací vzorků. Další chemické změny a podstata strukturních modifikací způsobené během teplotního působení byly interpretovány pomocí FTIR spektroskopie. (cs)
|
Title
| - FTIR spectroscopic and conductivity study of the thermal degradation of polyaniline films
- FTIR spectroscopic and conductivity study of the thermal degradation of polyaniline films (en)
- FTIR spektroskopická a vodivostní studie tepelné degradace polyanilinových filmů (cs)
|
skos:prefLabel
| - FTIR spectroscopic and conductivity study of the thermal degradation of polyaniline films
- FTIR spectroscopic and conductivity study of the thermal degradation of polyaniline films (en)
- FTIR spektroskopická a vodivostní studie tepelné degradace polyanilinových filmů (cs)
|
skos:notation
| - RIV/61389013:_____/04:00105805!RIV/2005/GA0/A55005/N
|
http://linked.open.../vavai/riv/strany
| |
http://linked.open...avai/riv/aktivita
| |
http://linked.open...avai/riv/aktivity
| - P(GA202/02/0698), P(IAA4050313), Z(AV0Z4050913), Z(MSM 113200001)
|
http://linked.open...iv/cisloPeriodika
| |
http://linked.open...vai/riv/dodaniDat
| |
http://linked.open...aciTvurceVysledku
| |
http://linked.open.../riv/druhVysledku
| |
http://linked.open...iv/duvernostUdaju
| |
http://linked.open...titaPredkladatele
| |
http://linked.open...dnocenehoVysledku
| |
http://linked.open...ai/riv/idVysledku
| - RIV/61389013:_____/04:00105805
|
http://linked.open...riv/jazykVysledku
| |
http://linked.open.../riv/klicovaSlova
| - polyaniline;conducting polymer;thin films (en)
|
http://linked.open.../riv/klicoveSlovo
| |
http://linked.open...odStatuVydavatele
| |
http://linked.open...ontrolniKodProRIV
| |
http://linked.open...i/riv/nazevZdroje
| - Polymer Degradation and Stability
|
http://linked.open...in/vavai/riv/obor
| |
http://linked.open...ichTvurcuVysledku
| |
http://linked.open...cetTvurcuVysledku
| |
http://linked.open...vavai/riv/projekt
| |
http://linked.open...UplatneniVysledku
| |
http://linked.open...v/svazekPeriodika
| |
http://linked.open...iv/tvurceVysledku
| - Stejskal, Jaroslav
- Trchová, Miroslava
- Šeděnková, Ivana
- Tobolková, E.
|
http://linked.open...n/vavai/riv/zamer
| |
issn
| |
number of pages
| |